Cork Peanut Massage Ball — 65 × 135 mm, Made to Your Density and Logo
Customizable density to match your product requirements.
Precision pressing for a consistent shape and structure.
Smooth sanding for a refined surface finish.
Custom logo engraving available.
MOQ: 300 pcs.
Description
Technical Parameters

Six numbers, if you only have ten seconds
| Material | Agglomerated cork - granulate plus PU binder, no wax or lacquer |
| Diameter × length | 65 mm × 135 mm, tolerance ±1.0 mm on both |
| Density | 380 kg/m³ standard, 300–450 kg/m³ on request |
| Logo | Laser engraving, or screen print above 500 pcs |
| MOQ | 300 pcs customized · 100 pcs stock spec |
| Lead time | Sample 5–7 days · Bulk 18–25 days |
Full specification
| Material | Agglomerated cork, 2–4 mm granulate, PU binder, natural color, no dye |
| Standard size | Ø 65 mm × 135 mm (two Ø 65 mm balls joined at a 40 mm waist) |
| Other sizes we press | Ø 45 / 55 / 75 mm single ball · length 90 / 120 / 150 mm peanut |
| Tolerance | Diameter ±1.0 mm · Length ±1.5 mm · Roundness 0.8 mm max |
| Density | 380 kg/m³ standard; 300 / 340 / 420 / 450 kg/m³ available. Density tolerance ±5% |
| Unit weight | ≈110 g at 380 kg/m³ · ≈130 g at 450 kg/m³ (Ø 65 × 135 mm). Weight follows density - order by density, not by gram, or the two will not match |
| Surface | Sanded at 80–120 grit. No wax, oil, or lacquer - those polish the face and it stops gripping when wet |
| Moisture content | ≤ 7% at packing, measured per batch |
| Waist joint | Pressed in one peanut-shaped cavity - no bonded seam |
| Logo method | Laser engraving (standard) · screen print (1–2 colors, above 500 pcs) |
| MOQ | 300 pcs with your logo or your density · 100 pcs for our stock spec |
| Sample lead time | 5–7 days for our standard spec · 10–12 days for a new density or size |
| Bulk lead time | 18–25 days after artwork and density approval |
| Monthly capacity | 26,000 pcs on this line (5 pressing stations × 1,000 pcs/day); 500,000 across all cork lines |
| Packing | 50 pcs per poly bag, 100 pcs per carton, carton 52 × 38 × 34 cm, 13 kg gross at 380 kg/m³ |
| Pallet | 40 cartons per pallet, 1,000 × 1,200 mm, shrink-wrapped |
| HS code | 9506.91 |
| Port of loading | Qingdao / Shanghai, FOB |
| Payment terms | T/T 30% deposit, 70% against copy of B/L |
| Compliance | No CE marking is claimed - cork massage balls fall outside the scope of the EU CE directives. Material and process records are handed over per order; name the specific document your compliance file requires and we will tell you exactly what we can provide. |

Tell us the use case, we tell you the density
Most buyers ask for "a cork ball" and then discover the firmness is wrong for their customer. Density is the variable that decides firmness - size only decides coverage. Use the left column, not the middle one, when you write your RFQ.

| If your program is… | Ask for | Why |
|---|---|---|
| Studio or retail entry SKU, mainstream adults | Ø 65 × 135 mm, 380 kg/m³ | The middle density. Firm enough to reach the erector spinae, soft enough that a first-time user does not bruise |
| Physical therapy or sports recovery channel | Ø 65 × 135 mm, 420–450 kg/m³ | Higher density gives a slower, more controlled roll and less surface give on large muscle groups |
| Beginner, senior, or sensitive-area programs | Ø 55 mm single ball, 300 kg/m³ | Smaller contact area under lower load. Cork may still be too firm - see the honest note below the table |
| Foot, forearm, and small muscle groups | Ø 45–55 mm single ball | Peanut geometry does not help where the muscle group is narrower than the waist |
| Other | Send a drawing, a photo, or one physical sample. We confirm geometry and density before we open a mold - no sampling charge if we cannot hit your spec. | |
Cork is not automatically the right answer
| Type | Best for | Cost | What you need to know |
|---|---|---|---|
| Agglomerated cork (this product) |
Brands selling the material story; hot yoga; buyers who want a natural surface that grips when damp | Highest of the four | Heavier per unit - expect real freight cost on air shipments. Color varies between harvests, so batch-to-batch match is a range, not a constant. Low-density cork crumbles; density is not a place to save money |
| Solid natural cork | Nothing at this size | 3–5× agglomerated | A 65 mm solid block has to be bored out, and the waste is most of the block. We do not offer it and would not recommend it for a double ball |
| EVA foam | High-volume, low-price, soft-touch programs | Lowest | Compresses permanently within months of daily studio use. Takes on sweat odor and cannot be washed out. No material story to sell |
| TPR / rubber | Deep-pressure work where hardness is the point | Mid | Petroleum-based, so it cancels whatever sustainability angle your brand is built on. Noticeable odor on opening a sealed carton |

What your logo actually looks like on cork
Laser engraving
Laser engraving
The beam burns the cork surface to a dark brown. It cannot peel, chip, or wash off, and it survives the whole life of the ball. This is what we recommend for anything above 300 pcs.
Screen print
Water-based ink, opaque, holds fine detail and brand color better than laser. Good for retail packaging where the logo has to match a style guide.
Custom density and size
A new mold for a new geometry, or an existing mold at a different fill weight for a different density. Density changes are cheaper and faster than geometry changes.
Six things that show up after the container arrives
Six failures, roughly in the order they surface. You cannot see any of them in the sample photo you approve, and none of them is exotic - they are ordinary in this category. What separates one supplier from another is whether anyone can name the cause before you have to name the complaint.
1. The second batch is softer, and nothing on the box says so
The complaint arrives months after the invoice. Your distributor's customer bought a peanut ball in spring, buys another one now, and says the new one feels soft. Both were pressed at 380 kg/m³. Both passed inspection. Neither fact helps her.
Firmness is not a material property here. It is arithmetic. Granulate goes into a closed cavity by volume, so density is the weight you poured in divided by a cavity that never moves. Drift the dosing scale by 2 g on a 110 g ball and density has moved 1.8% - and no gauge on the line flags it, because a ball that is 2 g light looks exactly like a correct one.
We spent a year blaming the press for that. The press was fine. A press either closes or it doesn't. A scale drifts a little every morning, and nobody notices.
So every batch is weighed and logged against the approved reference, and density is held to ±5%. The reference ball sits on the QC bench as a physical object rather than a photo. A photo cannot be squeezed.
Ask for: the fill-weight log for your batch and the density figures for the two batches before it. Three numbers within 5% of each other, or do not take the shipment.
2. Brown dust in the bag, and it is not packing dust
A cutter opens a carton on the pallet and finds brown powder in the folds of the bag, a few loose granules rattling at the bottom. It reads as packing dust. It is the outside of the ball coming apart.
Agglomerate is granules held by binder that has cured around each one. That matrix is thinnest exactly where the granulate pressed hardest against steel, at the mold face. Abrade that face on cotton or a mat for a few hundred hours and the under-bonded granules let go. In a studio the result is a brown smear on the floor and your logo on the customer's mat.
More binder is the obvious answer and the wrong one: it makes the ball feel plastic. What works is dosing the binder tightly, curing at temperature rather than in ambient air, and sanding the mold face after demolding so the customer touches well-bonded core instead of starved skin. We sand at 80–120 grit for that reason, and every batch sends 5 balls through an abrasion check: 500 g load, 100 strokes on cotton, under 0.3 g lost.
Test it yourself: one ball, one kitchen scale, an hour of rubbing it on denim. If the number moves enough to read without squinting, we shipped the wrong batch.
3. The soft spots had nothing to do with the binder. We changed suppliers twice learning that
Roughly one ball in fifty. Always the same place on the waist, always with a faint smell to it. Our first answer was the glue. We changed suppliers. The soft spots came back. We changed again. They came back.
It was water. Granulate in a wet month arrives at 10–14% moisture. Close a mold on that and the water flashes to steam, so the press pushes back against a gas instead of a solid, the same fill weight occupies more volume, and that patch comes out light. The steam also cools the binder before it finishes curing, so the same patch is weak. One cause, two defects, neither visible from outside.
Granulate is dried to ≤7% before blending now, and moisture is measured on every incoming lot instead of once a month. In a wet season that costs a day of throughput. It cost less than the returns did.
One question sorts this out: what was the granulate moisture on the lot used for our order, and when was it measured? Someone who has thought about this answers in ten seconds. Someone who hasn't will tell you about their certifications instead.
4. One millimetre out of round and the whole thing feels cheap
±1.2 mm. That is the deviation at which a double ball stops tracking.
Under it, the ball goes where you push it. Over it, one half carries more mass, the ball walks sideways, the user's hand corrects on every stroke, and a release technique turns into a wobbly toy. Nobody writes roundness deviation in a review. They write it doesn't roll properly, and your brand absorbs it.
Roundness is set by the cavity and by how the ball leaves it. Sanding cannot rescue an oval ball, because sanding makes a small ball, not a round one. Cavities are gauged against a master every 5,000 shots and pulled at 0.6 mm; finished balls are held to 0.8 mm, with diameter and length specified two-sided at ±1.0 and ±1.5 mm. A one-sided 65 mm tells your incoming inspector nothing about what her calipers are allowed to read.
Three balls, one flat table: push them away from you. Straight tracking means the mold is sound. A curve means box it up with the batch number and we will tell you which cavity it came out of.
5. The reorder was never going to match, because nobody wrote the first one down
That sentence is usually not a quality complaint. It is a filing complaint.
Order one ran on one granulate lot, one grit, one laser power, and all three of those lived in an operator's head. Six months later someone else runs the reorder. The ball comes out a shade darker and slightly glossier, every measurement inside the spec, and your distributor calls it a different product. From where they stand, it is.
Paper does not fix this. A signed physical standard does. Before bulk we send you the approved ball and seal an identical one in the QC room, labelled with batch number, density, grit and laser settings. Reorders get checked against that ball held in a hand, not against a document. We keep them 24 months.
On your second order: ask for the sealed reference ball from the first. If we cannot put it in a box and mail it to you, the matched-reorder promise was marketing and you should price it that way.
6. Cork has no smell. The binder does.
A container that crossed an ocean in August opens with a tire-shop smell. It fades in a day or two. It should not have been there at all.
Polyurethane binder keeps releasing a little residual monomer and solvent after the press, and three weeks in a sealed steel box at container temperature pushes it out of the ball. Cork makes that worse in its own way: it absorbs odor easily and gives it back slowly, so the smell reaches your customer's nose days after the retail carton opens, which is precisely when they are deciding whether to trust the brand on the box.
The mistake is packing off the press. Ours rest 72 hours in a ventilated curing room, and no batch is released until a panel has smelled it against a reference ball. Bags are vented rather than sealed, which costs a little per unit and does more for this complaint than anything else we have tried.
Ask for one number: the curing-room dwell time, in hours. Under 48 and those balls went into the bag while they were still curing.
Who buys this, and in what configuration

Two contact points either side of the spine, waist clearing the vertebrae between them. That geometry is the entire reason this shape exists.
Yoga and Pilates studios - sold as a prop alongside mats and blocks; usually the studio's own label, low logo complexity. Typical: Ø 65 × 135 mm, 380 kg/m³, laser logo, 300–500 pcs
Fitness retail and e-commerce brands - a single-SKU recovery item, so packaging and shelf presence matter more than the spec sheet. Typical: Ø 65 × 135 mm + printed box, 1,000–3,000 pcs
Physical therapy and rehab suppliers - the buyer is a clinician and will read the tolerance and density rows before anything else. Typical: Ø 65 × 135 mm, 420–450 kg/m³, tight tolerance, 500 pcs
Corporate wellness and gifting - one seasonal drop, brand colors on the box, engraving on the ball. Typical: 500–1,000 pcs, single delivery date
Sports team and recovery-kit assemblers - combined with rollers and bands in one kit, so unit weight and carton cube drive the decision. Typical: Ø 55 mm, kit-packed
From your drawing to your first sample: 10–12 days
Day 0 - you send a drawing, a photo, or a physical sample, plus the density you think you want and the quantity.
Day 1 - we confirm geometry, density, logo method, and price in writing. If we think a different density serves you better, we say so here, not after the deposit.
Day 2–3 - you approve. Deposit received. Production slot is locked for the date we quoted.
Day 4–12 - sample pressed, sanded, engraved, photographed, and shipped by express at your account or ours.
Sample approved - we seal the reference ball, and the bulk run is compared against that physical ball, not against a photo.
Day 18–25 - bulk ready, pre-shipment photos and the QC records sent before the cartons are loaded.
The carton figures in the specification table are for our standard poly-bag packing. Change the inner packing and the carton count changes with it, so confirm the packing method when you enquire. Mold cost for a new geometry and printed-box cost are quoted against your drawing or artwork - charged once, sent with the quotation.
All of the above assumes there is actually a plant behind it
Xi'an Tianlei Rubber Technology Co., Ltd. has been pressing cork since 2007, on a 22,000 m² site with 12,000 m² of building and more than 15 production lines. We make cork coasters, stoppers, covers, and cork yoga and fitness products, and we export to more than 40 countries. That is not a claim about quality - it is a claim about capacity and about who is answering your email.
2007Established
22,000 m²Plant site
5Pressing stations
26,000Pcs / month, this line
40+Countries
15+Production lines

Diameter and roundness go against a master gauge, every batch. Nobody photographs this step, which is roughly why it is worth asking a supplier for.
Address: No.3, Tuanjie Rd., Ind. Park, Caotang Town, Xigao New Huyi Dist., Xi'an, Shaanxi, China. Visitors are welcome - tell us two days ahead and we will have the reference samples and your counter-samples on the bench.
Questions buyers actually send us
Is this a solid piece of cork or pressed granulate?
Pressed granulate - cork granules at 2–4 mm bound with PU binder, molded in one peanut-shaped cavity. Solid cork at this size would have to be bored from a block, would weigh considerably more, and would cost three to five times as much. If your spec says "solid cork," tell us early, because we will decline the order rather than ship granulate and let you find out.
Does the surface get slippery when you sweat on it?
No - it gets grippier. Cork's cell structure swells slightly with moisture, which increases friction. That is why we refuse to wax or lacquer the surface even when a buyer asks for a "smoother finish": polishing closes the cells and the property reverses. We sand at 80–120 grit and stop there.
What is the MOQ, and does it change with customization?
300 pcs with your logo, your density, or your packaging. 100 pcs if you take our stock specification with no logo. A new mold is separate and does not consume the MOQ.
Can I get a sample before ordering, and who pays the freight?
Yes. Samples of the standard spec are free; you pay the courier, or give us your account number. A sample in a new density or a new size is quoted with your enquiry. Sample time is 5–7 days for standard and 10–12 days for a new spec.
How long is bulk production?
18–25 days after you approve artwork and density. In the August–October peak the figure moves to 25–30 days, so place the order earlier if your launch date is fixed. We would rather tell you the real number than promise 20 days and ship late.
Is there a price break, and can you give me a range now?
Three tiers: 300–999, 1,000–4,999, 5,000+. We quote exact FOB numbers rather than a published range, because density and packaging change the cost more than quantity does. Send quantity, density, and logo method and you will have a number within 24 hours.
What are the limits on the logo?
Laser engraving: single color, always dark brown, minimum stroke 0.8 mm, minimum type height 4 mm, no white or metallic. Screen print: 1–2 colors, above 500 pcs, edge bleed 0.3–0.5 mm so no hairlines or small reversed type. We send a photo of your artwork on your actual granulate before the bulk run - approve that photo, not a vector mockup.
Can I choose the density?
Yes, within 300–450 kg/m³. Below 300 the bond matrix is too sparse and the ball sheds granulate - if that is your target, tell us early and we will say so before you commit. Above 450 the ball becomes brittle at the waist and chips. Both ends of that range are real limits, not sales framing.
Will the color match between orders?
Not exactly, and no supplier can promise it. Cork granulate color shifts with each harvest, so batch-to-batch difference is a range rather than a constant. We send the granulate lot photo with your pre-shipment photos so you can see it before the container leaves. If your brand depends on exact color match, cork is the wrong material and we will say so.
What happens if part of a batch is defective?
Every carton carries a batch number, so a problem can be traced back to a specific pressing run rather than argued about. Send photos and that number. What we do next depends on which of the three failure modes it is - dimensional, bonding, or density - because each has a different cause and a different fix: a credit for a density miss, a replacement run for a bonding failure, a cavity check for a roundness complaint. The claim window, the threshold between a credit and a replacement, and who covers return freight are written into the proforma invoice for each order, so they are agreed before production instead of being discovered afterwards. We would rather set them per order than publish one figure here that cannot fit both a 300-piece trial and a 20,000-piece program.
What certifications do you have?
We do not display a certification logo unless we can send you the certificate number alongside it, and for this product we currently cannot - so we are not claiming ISO 9001, ISO 14001, FSC, or CE here. On CE specifically: cork massage balls fall outside the scope of the EU CE directives, so a CE claim would be meaningless even if we printed one. What we can hand over with a quotation is the evidence behind every number on this page - fill-weight logs, abrasion results, roundness checks, and the sealed reference ball. If your own compliance file needs a REACH SVHC report on the granulate and the binder before you can list the product, name it in the RFQ. We can arrange that test, and we would rather quote it than imply we already hold it.
Do you make any therapeutic claims?
No, and we would advise you not to either. This is a fitness and recovery accessory, not a medical device. Claims about relieving chronic pain, treating sciatica, or aiding injury recovery will put a retail listing into a regulated category and can trigger a substantiation request. Our page describes what the product is and what it is made of; what it does for a specific user is for their doctor to say.
Hot Tags: Cork Peanut Massage Ball — 65 × 135 mm, Made to Your Density and Logo, China Cork Peanut Massage Ball — 65 × 135 mm, Made to Your Density and Logo manufacturers, suppliers, factory, Cork Yoga Block, Natural Cork Tile, Cork Yoga Mat Block, Massage Roller Cork, Natural Cork Tiles, Cork Natural Rubber Yoga Mat Cork
Previous
Cork Yoga Mat NaturalSend Inquiry